15-5pH po'lat qotishmasi 17-4 PH dan yuqori qattiqlikka ega bo'lishi uchun mo'ljallangan.15-5 qotishma tavlangan holatda martensitik tuzilishga ega va nisbatan past haroratli issiqlik bilan ishlov berish orqali yanada mustahkamlanadi, bu esa qotishmada mis o'z ichiga olgan fazani cho'ktiradi.15-5 ba'zi spetsifikatsiyalarda XM-12 deb ham ataladi
C | Cr | Ni | Si | Mn | P | S | Cu | Nb |
≤0,07 | 14,0-15,5 | 3,5-5,5 | ≤1,0 | ≤1,0 | ≤0,04 | ≤0,03 | 2,5-4,5 | 0,15-0,45 |
Zichlik | Elektr qarshiligi | Maxsus issiqlik quvvati | Termal kengayish koeffitsienti |
7.8 | 0,98 | 460 | 10.8 |
Vaziyat | bb/N/mm2 | b0,2/N/mm2 | d5/% | ψ | HRC | |
Yog'ingarchilik | 480 ℃ qarish | 1310 | 1180 | 10 | 35 | ≥40 |
550 ℃ qarish | 1070 | 1000 | 12 | 45 | ≥35 | |
580 ℃ qarish | 1000 | 865 | 13 | 45 | ≥31 | |
620 ℃ qarish | 930 | 725 | 16 | 50 | ≥28 |
AMS 5659, AMS 5862, ASTM-A564 (XM-12), BMS 7-240 (Boeing), W.Nr./EN 1.4545
•Yog'ingarchilikning qattiqlashishi
•Yuqori kuch
•600 ° F gacha o'rtacha korroziyaga chidamlilik
•Aerokosmik ilovalar
•Kimyoviy va neft-kimyoda qo'llanilishi
•Pulpa va qog'oz
•Oziq-ovqat mahsulotlarini qayta ishlash