MP35N - magnit bo'lmagan nikel va kobalt xromli molibden qotishmasi.Yuqori kuchlanish kuchi, 300ksi [2068MPa] gacha) yaxshi egiluvchanlik mustahkamligi va korroziyaga chidamliligi Vulkanizatsiyaga, yuqori haroratli oksidlanishga va vodorodning mo'rtlashishiga mukammal qarshilik. Noyob ko'rsatkich ishning qattiqlashishi, faza o'zgarishi va qarish jarayonidir.To'liq qotib qolgan holda ishlatilsa, ish harorati -200 ni tashkil qiladi~315°C va tavsiya etilgan maksimal harorat 750 daraja Farengeyt (399 daraja)
C | Mn | P | S | Si | Cr | Ni | Mo | Co | Ti | B | Te |
≦ 0,03 | ≦ 0,15 | ≦ 0,015 | ≦ 0,010 | ≦ 0,15 | 19,0 21,0 | 33,0 37,0 | 9,0 10,50 | ≧ 35,0 | ≦ 1,0 | ≦ 0,01 | ≦ 1,0 |
Zichlik (g/sm3) | Erish nuqtasi (°C) | Kengayish koeffitsienti (m/(m·°C)(21-93°C)) |
8.43 | 1440 | 12,8×10E-6 |
Vaziyat | sb MPa | s0.2 MPa | φ % | Ψ % | Qattiqlik HRC |
Qattiq eritma + Sovuq ish | 1758 | 1551 | 12 | 50 | 45 |
Qattiq eritma + Sovuq ish + Qarish | 1792 | 1585 | 8 | 35 | 38 min |
AMS5758, AMS5844, AMS5845, ANSI/ASTM F562, NACE MR0175
•Vulkanizatsiyaga yaxshi qarshilik, yuqori haroratli oksidlanish, tiniq, tuzli tuman va eng ko'p mineral kislotalar.
•Qattiq muhitda stressli korroziya yorilishiga yaxshi qarshilik va yuqori quvvat.
•Mahalliy korroziyaga yuqori qarshilik, masalan, chuqur korroziya va yoriq korroziyasi.
MP35N qotishmasi tibbiy davolanish, dengiz suvi, neft va gaz quduqlari, kimyo va mahkamlagich, bahor,
Oziq-ovqat mahsulotlarini qayta ishlash muhitining magnit komponentlari va uskunalari qismlari